Mapping of minority carrier diffusion length and heavy metal contamination with ultimate surface photovoltage method

Published online by Cambridge University Press:  15 July 2004

J. Lagowski
Affiliation:
Semiconductor Diagnostics Inc. 3650 Spectrum Blvd. #130, Tampa, FL 33612, USA
A. Aleynikov
Affiliation:
Semiconductor Diagnostics Inc. 3650 Spectrum Blvd. #130, Tampa, FL 33612, USA
A. Savtchouk
Affiliation:
Semiconductor Diagnostics Inc. 3650 Spectrum Blvd. #130, Tampa, FL 33612, USA
P. Edelman*
Affiliation:
Semiconductor Diagnostics Inc. 3650 Spectrum Blvd. #130, Tampa, FL 33612, USA
Get access

Abstract

The Ultimate surface photovoltage method of minority carrier diffusion length measurements reffered to as Ultimate SPV, replaces a sequential “one wavelength at a time” approach with simultaneous illumination with the entire set of wavelengths. In this multiwavelength beam, each monochromatic component is chopped with slightly different frequency. This enables simultaneous monitoring of all component SPV signals corresponding to different wavelengths using multi-frequency signal processing. The amplitude and phase of each component signals are then analyzed and used to calculate the diffusion length and surface lifetime. In-flight Ultimate SPV measurement, whereby the wafer continuously moves under SPV probe, is used for fast whole wafer mapping. In addition to speed advantages, Ultimate SPV offers a fundemental accuracy advantage due to elimination of differences in wafer condition during sequential illumination with individual wavelengths. High-speed measurements make it possible to add additional wafer treatments and perform multi-mapping required for separation of Fe and Cu in the silicon bulk. Wafer mapping in time of 2 minutes realized with Ultimate SPV is critical for monitoring of cobalt in silicon.

Keywords

Type
Research Article
Copyright
© EDP Sciences, 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

G. Zoth, in Recombination Lifetime Measurements in Silicon, edited by D. C. Gupta, F. R. Bacher, W. M. Hughes (ASTM STP1340, West Conshohocken, 1998), p. 30
J. Lagowski, P. Edelman, V. Faifer, ibid. p. 125
A. M. Goodman, J. Appl. Phys. 32, 2551, (1961)
J. Lagowski, United States Patent 5, 025, 145 and 5, 177, 351 (1991 and 1993)
Lagowski, J., Edelman, P., Erickson, R., Inst. Phys. Conf Ser. 144, 91 (1996)
Lagowski, J., Kontkiewicz, A. M., Jastrzebski, L., Edelman, P., Appl. Phys. Lett. 63, 2902 (1993) CrossRef
J. Lagowski, A. Aleynikov, V. Faifer, United States Patent 6, 512, 384 (January 28, 2003)
Lagowski, J., Edelman, P., Kontkiewicz, A. M., Milic, O., Henley, W., Dexter, M., Jastrzebski, L., Hoff, A. M., Appl. Phys. Lett. 63, 3013 (1993)
N. Pic, M. L. Polignano, D. Caputo, G. Salva, M. Sardo, A. Danel, in Proceedings of the Electrochemical Society Fall Meeting “High Purity Silicon” (PV 2003-03, October 2002), p. 505