Hostname: page-component-8448b6f56d-xtgtn Total loading time: 0 Render date: 2024-04-19T14:54:59.793Z Has data issue: false hasContentIssue false

Electrical Characteristics of LSMCD-Derived SrBi2.4Ta2O9 Thin Films Using TiO2 Buffer Layer for Metal/Ferroelectric/Insulator/Semiconductor Field Effect Transistor Devices

Published online by Cambridge University Press:  10 February 2011

Joo Dong Park
Affiliation:
Department of Metallurgical Engineering and Materials Science, Hong Ik University, Seoul 121-791, Korea
Tae Sung Oh
Affiliation:
Department of Metallurgical Engineering and Materials Science, Hong Ik University, Seoul 121-791, Korea
Get access

Abstract

Pt/SBT/TiO2/Si structure was proposed for metal/ferroelectric/insulator/semiconductor field effect transistor (MFIS-FET) applications. SrBi2.4 Ta2O9 (SBT) thin films of 400 nm thickness were prepared using liquid source misted chemical deposition (LSMCD) on Si(100) substrates with TiO2 buffer layers deposited by DC reactive sputtering with the thickness ranging from 5 nm to 200 nm and electrical properties of MFIS structures were investigated. Memory window and maximum capacitance of the Pt/SBT/TiO2 /Si structure increased with decreasing the thickness of TiO2 buffer layer. The Pt/SBT(400 nm)/TiO2(10 nm)/Si structure exhibited C-V hysteresis loop with the memory window of 1.6 V at ±5 V, and could be applicable for MFISFET applications.

Type
Research Article
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Scott, J. F. and Paz de Araujo, C. A., Science, 246, 1400 (1989).Google Scholar
2 Scott, J. F., Ferroelectrics Review, 1, 85 (1998).Google Scholar
3 Moll, J. L. and Tarui, Y., IEEE Trans. Electron Devices, ED-10, 338 (1963).Google Scholar
4 Shichi, Y., Tanimoto, S., Goto, T., Kuroiwa, K., Tarui, Y., Jpn. J. Appl. Phys., 33, 5172 (1994).Google Scholar
5 Kim, Y. T. and Shin, D. S., Appl. Phys. Lett, 71, 3507 (1997).Google Scholar
6 Lee, H. N., Kim, Y. T., and Choh, S. H., J. Kor. Phys. Soc., 34, 454 (1999).Google Scholar
7 Tokumitsu, E., Itani, K., Moon, B., and Ishiwara, H., Jpn. J. Appl. Phys., 34, 5202 (1995).Google Scholar
8 Alexsandrov, P., Koprinarova, J., and Todorov, D., Vacuum, 47, 1333 (1996).Google Scholar
9 Schroder, D. K., Semiconductor Materials and Device Characterization, 2nd ed. (John Wiely & Sons, 1998), Chap. 6.Google Scholar
10 McMillan, L. D., Huffman, M., Roberts, T. L., Scott, M. C., and Araujo, C. A. Paz de, Integrated Ferroelectrics, 4, 319 (1994).Google Scholar
11 Miller, S. L. and McWhorter, P. J., J. Appl. Phys., 72, 5999 (1992).Google Scholar