The Characteristics and Oxidation of Vapor - Liquid - Solid Grown Si Nanowires

Published online by Cambridge University Press:  15 February 2011

J. Westwater
Affiliation:
Sony Research Center, 174 Fujitsuka-cho, Hodogaya-Ku, Yokohama 240, Japan, jwestw@src.sony.co.jp
D. P. Gosain
Affiliation:
Sony Research Center, 174 Fujitsuka-cho, Hodogaya-Ku, Yokohama 240, Japan, jwestw@src.sony.co.jp
S. Tomiya
Affiliation:
Sony Research Center, 174 Fujitsuka-cho, Hodogaya-Ku, Yokohama 240, Japan, jwestw@src.sony.co.jp
Y. Hirano
Affiliation:
Sony Research Center, 174 Fujitsuka-cho, Hodogaya-Ku, Yokohama 240, Japan, jwestw@src.sony.co.jp
S. Usui
Affiliation:
Sony Research Center, 174 Fujitsuka-cho, Hodogaya-Ku, Yokohama 240, Japan, jwestw@src.sony.co.jp
H. Ruda
Affiliation:
Department of Metallurgy and Materials Science, University of Toronto, 184 College Street, Toronto, Canada M5S 3E4
Get access

Abstract

The Vapor - Liquid - Solid (VLS ) technique allows the growth of high aspect ratio Si wires. The Si nanowires formed by this technique can be thinned down by oxidation. This approach allows the formation of very thin Si cores which may be used to research the properties of Si nanostructures. In this work the growth and oxidation of these wires is characterized.

In the growth a very thin layer of Au is deposited on a Si (111) surface, silane gas is introduced into the chamber as the Si source gas and the temperature is raised to 300 – 600°C. Initially a catalytically active Au surface phase leads to the growth of a defective epitaxial Si layer. As Au / Si molten alloy balls nucleate and grow in size to approach the threshold size for VLS wire growth, which is determined by the Gibbs - Thomson effect, the epitaxial layer growth rate decreases and a transition to Si nanowire growth occurs. The morphology and width of the wires is strongly dependent on the growth temperature and pressure. At low pressure and high temperature relatively thick well-formed wires grow straight up from the substrate surface along the [111] direction. As the temperature is decreased and the pressure is increased thinner wires (as thin as 10 nm ) grow which tend to exhibit growth defects. A light oxidation yields Si cores which are of the order of 5 nm in diameter.

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1.Wagner, R.S. and Ellis, W.C., Appl. Phys. Lett., 4, 89 (1964).Google Scholar
2.Wagner, R.S. and Doherty, C.J., J. Electro. Chem. Soc, 115, 93, (1968).Google Scholar
3.Givargizov, E.I., J. Cryst. Growth, 31, 20 (1975).Google Scholar
4.Hiruma, K., Yazawa, M., Katsuyama, T., Ogawa, K., Haraguchi, K., Koguchi, M., and Kakibayashi, H., J. Appl. Phys., 77, 447 (1995).Google Scholar
5.Westwater, J., Gosain, D.P., Tomiya, S., Usui, S., and Ruda, H., submitted to J. Vac. Sci. Tech.Google Scholar
6.Lelay, G., Surface Science, 132, 169, (1983).Google Scholar
7.Binary Phase Diagrams, edited by Okamoto, H., Subramanian, P.R. and Kacprzak, L. (W.W. Scott, 1992 ), Vol. 1, 2nd edition.Google Scholar
8.Kao, D.B., McVittie, J.P., Nix, W.D., Saraswat, K.C., IIIE Trans. Elect. Dev., 34, no. 5, 1008, (1987).Google Scholar